TiAlN-high titanium
Property
Coating temp (℃):500
‧Nanohardness (GPa):30
‧Thickness (μm):1~4
‧Friction coefficient:0.5
‧Max usage temp (℃) :800
‧Coating structure:Nanocomposite Coating
Coating temp (℃):500
‧Nanohardness (GPa):30
‧Thickness (μm):1~4
‧Friction coefficient:0.5
‧Max usage temp (℃) :800
‧Coating structure:Nanocomposite Coating